1、氣溫:最好在5℃以上施工,溫度太低容易冷凝,不利涂膜的干燥,且會出現裂紋、水泡等情況;
1, the temperature: the best in the construction of more than 5 degrees Celsius, the temperature is too low easy to condensation, unfavorable film drying, and there will be cracks, blisters, etc.;
2、不能再結冰或上霜的基面上施工,也不要在低于4℃時使用。確實因工期必要必須施工時,可將施工時間安排在晴天好氣候的10:0-15:00之間,延續環境溫度低于零下4℃時,建議停息施工;
2, can not freeze or frost on the surface of the construction, do not contact the environment within 48 hours when the temperature is less than 4 degrees. Indeed, because of the need for the construction period, the construction time can be arranged in a sunny weather 10:0-15:00,When the ambient temperature is below 4 degrees below zero, it is recommended to suspend construction;
3、不宜在雨雪天施工,新施工的外觀固化前不要被雨淋。施工后48小時內(百度搜索引擎優化),仍應避免雨淋、霜凍貨0℃以下的長期低溫;在空氣流通不良或不具備透風條件的情況下(如封閉的礦井或隧道),可采用風扇或鼓風機幫忙透風。
3, not in the rain and snow surface construction, new construction is not cured before the rain. Within 48 hours after construction, should avoid long-term low temperature rain and frost goods 0 DEG C; in the case of poor air circulation or do not have ventilation conditions (such as closed mine or tunnel), can be used to assist the ventilation fan or blower.