原因分析 Reason:
(1)混凝土、砂漿施工質量不良,存在微孔滲透;
(1) the construction quality of concrete and mortar is bad;
(2)板面、隔墻出現輕微裂縫:
(2) the board, partition slight crack:
(3)屋頂防水涂層施工質量不好或損壞。
(3) poor quality or damage of waterproof coating.
堵漏措施 Plugging measures:
(1)拆除飾面材料,暴露滲水部位,涂刷屋頂防水涂料。除純丙烯酸屋頂防水涂料外,通常都要求配合防水聚酯布進行修補。
(1) removal of decorative materials, exposure to water seepage, coating waterproof coating. In addition to polyurethane waterproof coating, usually with fiber materials to repair.
(2)如有開裂征象,則應對裂縫進行加強屋頂防水處理;貼縫法:對細小的發絲裂縫,可刷屋頂防水涂料并加貼防水聚酯布,作屋頂防水處理;填縫法:若較顯明的裂縫,要進行擴縫處理(北京設計),將縫擴展成15 ×15mm左右的V型槽,在清理干凈后(河南人事考試),刮填屋頂防水涂料或嵌縫材料;填縫加貼縫:除采用填縫法處理外,在縫外觀再涂刷屋頂防水涂料,并粘貼防水聚酯布處理。亦可不拆除飾面,直接在其外觀刷涂純丙烯酸屋頂防水涂料。
(2) if there are cracks, cracks should strengthen waterproof treatment; mount joint method: tiny hair crack, can brush waterproof paint and add fiber material or cloth, waterproof treatment; filling method: if the crack is obvious, to enlarge the joint treatment, will be extended to V type groove joint about 15 * 15mm, in clean, scraping fill waterproof coating or caulking material; filling affixed by caulking seams: in addition to treatment, the joint surface waterproof coating is coated, and paste fiber material processing. Can not remove the surface, directly on the surface of transparent or colored polyurethane waterproof coating.